TIP TIG welding is 100 to 500% faster than TIG with superior quality than traditional TIG - Pulsed MIG - FCAW

TIP TIG Welding

 

TIP TIG Welding Videos 2



TIP TIG USA is responsible for TIP TIG sales in North & South America and Australia.
TIP TIG is located at The Philly Navy Yard. 1901 Kitty Hawk Ave.
Building 68 Philadelphia. PA. USA.



TIP TIG PROVIDES LESS WELD HEAT AND BETTER WELD QUALITY THAN TIG
AND PROVIDES THOSE WELDS AT MIG WIRE FEED RATES.



TIG Welding Brochure
Click on the Evolution of TIG icon if you want a TIP TIG brochure.





The owners of TIP TIG USA are Ed Craig and Tom O' Malley.
TIP TIG web site is www.tiptigusa.com. Call Ed 828 658 3574. Cell 828 337 2695.
E-mail ed@tiptigusa.com or tom@tiptigusa.com.



IF VIDEOS STALL REPLAY TWICE, BETTER SECOND TIME

 


Work that TIP TIG cup on that P91 root. "This weld is easy, it's my back pain that's the real issue. It sure helps to be able to steady myself with my left hand".


We can provide great weld quality but the video quality could be better.

This TIP TIG P91 pipe weld coupon fill just needs a little torch weave.

You can't beat this TIP TIG water cooled torch it's really light and it's nice to lean on the pipe like this, kinda relaxing.


Note the slow wire feed coming from the TIP TIG feeder, it's slow because it's a root, yet TIP TIG is still feeding the wire 100% faster than any welder can attain with traditional TIG. With TIP TIG, no time outs or smoke breaks for picking up a length of weld wire or weld starts / stops. With TIP TIG if the most difficult welds are made simple I guess the simple welds should look great.





This is one of the positions I use at Yoga. I bet now he is using TIP TIG he's glad his left hand is supporting him while he works his right hand and the TIP TIG weld






A BASIC WELD FACT. IT TYPICALLY TAKES TWO TO FOUR TIG
& SMAW WELDERS TO DO THE WORK OF ONE TIP TIG WELDER.


REGULAR TIG VERSUS TIP TIG WELD DEPOSITION DIFFERENCES.

This table represents the most common all position steels and alloy steel applications.

[1] Pipe Root
Regular Manual TIG
wire feed rate.

10 inch/min

(70 inch/min)

Manual TIP TIG
wire feed rate increase.


25 - 50%
[2] Pipe Fill

Wall < 3/8 (a)
10 inch/min

(70 inch/min)

100 - 200%
[3] Pipe Fill

Wall > 3/8
10 inch/min

(70 inch/min)
100 - 300%
[4] 1/8 Fillet
10 inch/min

(70 inch/min)
100 - 200%
[5] 3/16 Fillet
Great setting also for all position cladding
10 inch/min

(70 inch/min)
> 150%
[6] 1/4 Fillet
10 inch/min

(70 inch/min)
200 to 400%


Note: Red is conversion from 3/32 2.4 mm wire to 0.035 0.9 mm wire.
5G pipe weld figures are real world. You will have some TIG welders that will
deposit slightly more weld wire and there will be TIP TIG welders that
can provide higher wire feed rates. TIP TIG rates will increase with automation.



TO VIEW TIP TIG AT OUR PHILADELPHIA NAVAL YARD FACILITY
CALL ED FOR AN APPOINTMENT 828 337 2695.







ED'S MANUAL AND ROBOT WELD PROCESS CONTROL RESOURCES.

ED OPTIMIZED ROBOT WELDS FOR HUNDREDS OF COMPANIES. A FEW OF HIS PROJECTS,
FORD F150 FRAME - VOLVO CAB - CORVETTE FRAME- HARLEY FRAME - NEW BEETLE SEATS
AND THE ROBOT WELDS ON THE WORLD'S LARGEST CATERPILLAR TRUCK.









From optimizing and providing welding patents for automated, boiler water wall, pulsed MIG inconel clad welds for Welding Services Atlanta, to setting the robot welds on many of the most popular products sold in North America, if you want the training and educational resources to enable Best Weld Practices / Process Controls and optimize your manual / robot MIG and flux cored weld quality and productivity click here for Ed's materials.




For more TIP TIG data on the patent pending TIP TIG weld process
contact Ed Craig USA. Eastern Time. 828 658 3574.
E-Mail ed@tiptigusa.com or Tom O'Malley tom@tiptigusa.com.



To find out more on controlling manual and robot gage welds, MIG short circuit,
spray, pulsed MIG or flux cored, click on "Ed's Training Resources.






Next TIP TIG Weld Videos | Previous Videos | TIP TIG VS TIG Weld | TIP TIG Weld Pictures


TIP TIG Welding Home || Weld Reality Home

Site Established 2001. Ed Craig Weld Reality. E-Mail ecraig@weldreality.com. Phone Eastern Time USA 828 658 3574.